Erie Bronze & Aluminum Logo LadleFoundry FloorAluminum CastingsMoulds

Proprietary Process

Our proprietary degassing and static casting processes eliminate trapped gasses from the molten metal and assure uniform distribution of tin throughout the entire 850 and 852 casting. All metals are alloyed and tested in-house using an optical emission spectrometry (OES) Spectrometer. Optional test bars and chemistry reports are available to meet the customer’s QS and ISO requirements.


Degassing virtually eliminates porosity in the casting.

aluminum castings

Natural porosity of molten aluminum before and after degassing.

 

Most of the tubes produced are rough machined as ordered.  Aluminum alloys 850 and 852 can be heat treated to T5 condition.


Photo Gallery
Sand Casting Machined bottle mould with glass bottle
CastingCues
CastingCues are helpful tips to improve design & production of castings
Spanish, German,Chinese...
We Accept
Accepted Credit Cards

Photo Gallery
Sand Muller Machined Bottom Plate
CastingCues
CastingCues are helpful tips to improve design & production of castings
Spanish, German,Chinese...
We Accept
Accepted Credit Cards